Business Type:
Manufacturer/Factory
Establishment:
2012
R&D Capacity:
ODM, OEM, Other
OEM/ODM Service
Sample Available

ISO Tank, ISO Tank Container, Tank Container manufacturer / supplier in China, offering Anhydrous Liquid Ammonia Isotank Nh3 ISO Tank Container 20FT 24000L, 3 Axkes Liquid Ammonia Tank Trailer Pressure 2.49MPa Tank Volume 46000liters, Loading 23920K (NH3 Anhydrous Liquid Ammonia Gas), T20 Tank (UNPortable Tank) Un1838 - Cl4ti Titanium Tetrachloride 3220liters and so on.

1
    YRS
General Supplier

China HCl Acid Liquid Transport Tanks

Get Latest Price
Min. Order / Reference FOB Price
1 Piece US $12000.00/ Piece
Local Area: Wuhan, Hubei, China
R&D Capacity: OEM, ODM, Other
Payment Terms: LC, T/T, PayPal
Condition: New
Customized: Customized
Tank Marerial: Metal Tank
HCl Acid Liquid Transport Tanks (Hydrochloric Acid Tanks Acid Tanker Steel Lined PE Road Chemical Tank 16000L -17500L)
HCL Acid Liquid Transport Tanks for Truck lorry Customizing 5m3 - 25m3 ( Truck Mounted Tank body Carbon Steel inner Lined LLDPE )

metal cans Steel-Lined Plastic Transport Tank, Electrolytic Tank, Pickling TankCustom Made Rotationally Molded Linear Resins LLDPE
Custermizing Checmial Acid Transport Tank 1-150 m3 Steel Lined LLDPE Tank Used to Contain: HCl (max 35%) , Naoh (max 50%) , Naclo (max 10%) , PAC (max 17%) ,H2so4

Media (density) : (1155 Kg/m3), Hydrochloric Acid (1150 Kg/m3), Sulfate, Nitrate (1152 Kg/m3), Phosphate (1151 Kg/m3), Hydrofluoric Acid (1132 Kg/m3), Battery Fluid (1135 Kg/m3), Chloride (1135 Kg/m3), Ferric Chloride Solution (1130 Kg/m3), Sodium Hypochlorite (1130 Kg/m3), Sulfurous Acid (1030 Kg/m3)
processing/storing; aluminum sulfate, ammonium sulfate, calcium chloride, ethylene glycol, ferric chloride, ferric sulfate, ferrous sulfate, hydrochloric acid, hydrofluoric acid, hydrofluosilicic acid, hydrogen peroxide, magnesium chloride, phosphoric acid, polymers, potassium hydroxide, or just plain water and we'll design the Transport vessel(s) you require.
Transport HCL Acid Tanks Steel Lined LDPE
For Transport Bleach, Hydrochloric Acid, Ferric Chloride, Oilfield Chemicals, Corrosive Wastes And Other Hazardous Cargoes.
Steel ( 6 mm -8mm ) Lined PE Plastic 7042 (16mm - 25 mm ) Transport tank Steel Lined LDPE Tank Transport HCL(max 35%), NaOH (max 50%), NaCLO (max 10%), PAC (max 17%),H2SO4(60%,98%) ,HF (48%),H3PO4 (10%-85%),NH3. H2O,H2O2 (30%) Hazardous Liquids Transport Tank

Steel Lined LDPE aslo for Transport HCL(max 35%), NaOH (max 50%), NaCLO (max 10%), PAC (max 17%),H2SO4(60%,98%) ,HF ( 48%),H3PO4 (10%-85%),NH3. H2O,H2O2 (30%)
Compounds, cleaning liquid, UN1760,
Corrosive liquid, acidic, inorganic, n.o.s., UN3264,
Corrosive liquid, acidic, organic, n.o.s., UN3265,
Corrosive liquid, basic, inorganic, n.o.s., UN3266,
Hypochlorite solutions, UN1791,
Hydrochloric acid solution, UN1789,
Sulfuric acid, UN2796,
BATTERY FLUID, ALKALI UN 2797,

Detail Picture



Vertical Hydrochloric Acid Storage Tanks ,Dosing tank, Day tank 30cbm (30000L) Draft
Vertical Bleach Sodium Hypochlorite ,Acid Storage Dosing Tanks 10cbm (10000L) Draft
Vertical Bleach Sodium Hypochlorite ,Acid Dosing Tanks , measuring tank 5m3 (5000L) Draft
Vertical Bleach Sodium Hypochlorite ,Acid Dosing Tanks , measuring tank 2m3 (2000L) Draft
metering tankVertical HCl Storage Tanks 90cbm (90000L ,23775Gallon) Draft
Vertical Hydrochloric Acid Storage Tanks 50cbm (50000L) Draft
Vertical Hydrochloric Acid Storage Tanks 30cbm (30000L) Draft
Vertical Hydrochloric Acid Storage Tanks 15cbm (15000L) Draft
Vertical Hydrochloric Acid Storage Tanks 10cbm (10000L) Draft
Vertical Hydrochloric Acid Storage Tanks 5000L Draft
Rotationally Molded LLDPE TANK
chemical resistance of LLDPE Cell / :+8615271357675
www.truckinchina.comLDPE / HDPE Chemical Resistance Chart

The chemical compatibility of LDPE and HDPE on this chart is tested at 20°C: and 50°C: for 7 days and 30 days (if applicable) with constant exposure.

LDPE & HDPE resistance listed by chemical1.4-dioxaneLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows some effect after 7 days.AcetaldehydeLDPE / HDPE at 20°C: little or no damage after 30 days.
HDPE at 50°C: shows some effect after 7 days.
LDPE at 50°C: immediate damage may occur.Acetic Acid 5 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Acetic Acid, glacial 50%LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50 °C: immediate damage may occur.AcetoneLDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.Allyl AlcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Aluminum saltsLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Amino acidsLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.AmmoniaLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Ammonium carbonate saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Ammonium phosphateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Ammonium sulphateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Amyl chlorideHDPE at 20°C: shows some effect after 7 days.
HDPE at 50°C & LDPE at 20°C-50°C: immediate damage may occur.
Not recommended for continuous use.AnilineLDPE / HDPE at 20°C: little or no damage after 30 days.
HDPE at 50°C: shows some effect after 7 days.BenzeneLDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.Benzyl alcoholLDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.Boric acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.BromineLDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.Butyric acidLDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.Calcium chlorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Calcium hydroxide saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Carbon tetrachlorideHDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C & HDPE at 50°C: show some effect after 7 days.
LDPE at 50°C: not recommended.Chlorine 10% in waterLDPE / HDPE at 20°C: shows little or no damage after 30 days.
LDPE at 50°C: shows damage and is not recommended.ChlorobenzeneImmediate damage may occur.
Not recommended for continuous use.ChloroformLDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: immediate damage may occur.
Not recommended for continuous use.Chromic acid 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Chromic acid 50%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Citric acid 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.CresolHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage.
Not recommended for continuous use.CyclohexaneLDPE / HDPE at 50°C: immediate damage may occur.
LDPE / HDPE at 20°C: show some effect after 7 days.Diethyl ketoneLDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.DimethylsulfoxideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Ethanol 95%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Ethyl acetateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Ethyl benzeneHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage.
Not recommended for continuous use.Ethylene glycolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Ethylene oxideHDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C: and LDPE/ HDPE at 50°C: show some effect after 7 days.Ferric chlorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.FluorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.FluorineHDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C: shows some effect after 7 days.
Not recommended at 50°C.Formaldehyde 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Formaldehyde 40%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.GlycerolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.HexaneHDPE at 20°C: shows little or no damage after 30 days continuous use.
HDPE at 50 °C: shows some effect after 7 days.
LDPE not recommended at any temperature.Hydrochloric acid 20%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Hydrochloric acid 35%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Hydrochloric acid 5%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Hydrocyanic acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Hydrofluoric acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Hydrofluoric acid 4%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Hydrofluoric acid 48%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Hydrogen peroxide 3%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Hydrogen peroxide 30%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Isobutyl alcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Isopropyl alcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.KeroseneLDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE not recommended at 50°C, as immediate damage may occur.Lactic Acid 10 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Lactic Acid 90 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Lead acetateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.MethanolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Methyl ethyl ketoneImmediate damage may occur.
Not recommended for continuous use.Methyl propyl ketoneHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur.
Not recommended for continuous use.Methylene chlorideHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur.
Not recommended for continuous use.Mineral oilLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: may show immediate damage and is not recommended.n-amyl acetateLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows some effect after 7 days or constant exposure.n-butyl alcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Nitric acid 50 %LDPE at 20°C: shows little or damage after 30 days.
HDPE at 20°C & LDPE at 50°C: show effect after 7 days.
HDPE at 50°C: shows immediate damage and is not recommended.Nitric acid 70 %LDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.n-octaneLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Oleic acidHDPE at 20°C-50°C: little or no damage after 30 days.
LDPE at 20°C-50°C: shows immediate damage and is not recommended.Oxalic acidLDPE at 20°C: shows some effect after 7 days.
HDPE at 20°C and LDPE / HDPE at 50°C: shows little/ no damage after 30 days.OzoneLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.Perchloric acidLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.Perchloric ethyleneLDPE / HDPE at 20°C-50°C: show immediate damage.
Not recommended.PhenolLDPE / HDPE at 20°C-50°C: show immediate damage.
Not recommended.Phosphoric acid 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Phosphoric acid 85%LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows immediate damage and is not recommended.Phosphorous trichlorideLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: has no data available. HDPE at 50°C: shows some effect after 7 days.Potassium carbonateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Potassium hydroxide 5 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Potassium hydroxide concentratedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Potassium permanganateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Propylene glycolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.PyridineImmediate damage may occur.
Not recommended for continuous use.Salicylic acid, saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Silver acetateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Silver nitrateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Sodium carbonateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Sodium chloride, saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Sodium dichromateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Sodium hydroxide 1%LDPE at 20°C-50°C: shows little or no damage after 30 days.
HDPE at 20°C-50°C: shows some effect after 7 days.Sodium hydroxide 50%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Sodium hypochlorite 15%HDPE at 20°C-50°C: little or no damage after 30 days.
LDPE at 20°C: is suitable but at 50°C: shows some effect after 7 days.Sodium nitrateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Sodium sulphateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.SucroseLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Sulfuric acid 20%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Sulfuric acid 6%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Sulfuric acid 60%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.Sulfuric acid 98%LDPE at 20°C-50°C: shows little or no damage after 30 days.
HDPE at 20°C: shows effect after 7 days.
Not recommended for use at 50°C.Tannic acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.TetrahydrofuranLDPE / HDPE at 20°C: show some effect after 7 day of constant exposure.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.TolueneLDPE at 20°C: show some effect after 7 day of constant exposure.
HDPE at 20°C-50°C & LDPE at 50°C: show immediate damage.
Not recommended.Trichloracetic acidLDPE / HDPE at 20°C: show some effect after 7 day of constant exposure.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.TrichlorethaneImmediate damage may occur.
Not recommended for continuous use.Turpentine oilLDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.UreaLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.XyleneHDPE at 20°C: shows some effect after 7 day of constant exposure.
LDPE at 20-50°C and HDPE at 50°C: show immediate damage.
Not recommended.Zinc chlorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.